MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem HRJ-4047 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: HRJ-4047 phenolic resin is an unmodified, thermoplastic resin made from octyl-phenol and formaldehyde. It is compatible with natural and synthetic elastomers, including SBR, BR, IIR and IR.

Applications: HRJ-4047 is utilized to develop high tack levels in rubber compounds, especially in synthetic rubber which do not impart inherent tack, for tire construction and mechanical goods. A typical loading is 3-10 phr. HRJ-4047 commonly replaces hydrocarbon resins which would typically need three times the loading to impart the equivalent tack of HRJ-4047 phenolic resin.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Value 25 - 4225 - 42
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 92.0 - 101 °C198 - 214 °F
 
Descriptive Properties
AppearancePellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH388 / 315306

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.