MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt DISTITRON® 420 C Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Orthophthalic

Appearance: Neutral - Transparent

Main resin characteristics: Clear, unaccelerated

Main applications: To flexibilize rigid resins

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Solids Content 71 - 75 %71 - 75 %MT-CU001C
Brookfield Viscosity 950 - 1250 cP950 - 1250 cPsp 3 rpm 20; MT-CUT23V
 
Chemical PropertiesMetricEnglishComments
Acid Value 16 - 2316 - 23[mgKOH/g]; MT-CU001I
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 6.00 MPa870 psiISO 527
Elongation at Break 57 %57 %ISO 527
Tensile Modulus 0.0850 GPa12.3 ksiISO 527
 
Processing PropertiesMetricEnglishComments
Gel Time 6.00 - 10.0 min
@Temperature 25.0 °C
6.00 - 10.0 min
@Temperature 77.0 °F
Reactivity at 25°C + 0,5% Co 6% + 1,5% MEKP50; RS.08.G
Shelf Life 3.00 Month3.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm100 - 130°CRS.08.G; Reactivity at 25°C + 0,5% Co 6% + 1,5% MEKP50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9399 / 231994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.