Product Properties: AG-E550D has better compatibilities with a variety of additives and offers excellent and durable water and oil repellency on various types of textiles, particularly made by synthetic fibers. AG-E550D also impart excellent liquid repellency to various types of nonwoven.Information provided by AGC Chemicals Americas Inc. |