System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
UBE 1013NW8 Polyamide 6 (unreinforced)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Unreinforced
Material Notes:
Characteristic: Injection, standard viscosity, fast cycle. Property data reported dry as molded.
Information provided by UBE Industries, LTD
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
ISO 1183-3
Moisture Absorption
2.70 %
2.70 %
50% RH; UBE method
Linear Mold Shrinkage, Flow
0.012
cm/cm
@Thickness 3.00 mm
0.012
in/in
@Thickness 0.118 in
30x100x3t; UBE method
Linear Mold Shrinkage, Transverse
0.013
cm/cm
@Thickness 3.00 mm
0.013
in/in
@Thickness 0.118 in
30x100x3t; UBE method
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
120
120
ISO 2039-2
Hardness, Shore M
80
80
ISO 2039-2
Tensile Strength, Yield
85.0
MPa
12300
psi
ISO 527-1,2
Elongation at Break
20 %
20 %
ISO 527-1,2
Tensile Modulus
3.20
GPa
464
ksi
ISO 527-1,2
Flexural Strength
110
MPa
16000
psi
ISO 178
Flexural Modulus
3.20
GPa
464
ksi
ISO 178
Charpy Impact, Notched
0.500
J/cm²
2.38
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
JIS K6911
Dielectric Constant
3.5
3.5
IEC 60250
Dielectric Strength
20.0
kV/mm
508
kV/in
IEC 60243-1
Arc Resistance
119
sec
119
sec
ASTM D-495
Comparative Tracking Index
>=
600
V
>=
600
V
UL746A
Thermal Properties
Metric
English
Comments
CTE, linear
80.0
µm/m-°C
44.4
µin/in-°F
ISO 11359-2
Melting Point
215
-
225
°C
419
-
437
°F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)
175
°C
347
°F
ISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi)
66.0
°C
151
°F
ISO 75-1,2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PUBD9806 / 287269
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.