MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TPO D-6509
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Multi-Flex® A-6509 thermoplastic elastomer blend is designed to provide processors with cost effective compounds with excellent tear strength, tensile strength and high elongation. Multi-Flex® A-6509 features good injection molding and extrusion flow characteristics. Parison strength is excellent for blow molding applications. Pre-drying prior to processing is usually not necessary as with other thermoplastic elastomers.

Data provided by Multibase.

Key Words: Thermoplastic Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792-91
Linear Mold Shrinkage 0.018 cm/cmASTM D955-89
Melt Flow 9.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6510 sec; ASTM D-2240-95
Tensile Strength, Ultimate 9.00 MPaASTM D638-95
Elongation at Break 1700 %ASTM D638-95
Izod Impact, Notched NBASTM D-256-93a
Tear Strength 47.3 kN/mASTM D624-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 685A10 Polyester Type Polyurethane Elastomer
Dow INFUSE™ 9817 Olefin Block Copolymer
Kraton® D1113 P (SIS) Linear Block Copolymer
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend
Multibase Multi-Flex® TPE A 8103 BLK

PLA234 / 49631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.