Physical Properties | Metric | English | Comments |
---|
Density | 1.478 - 1.492 g/cc | 0.05340 - 0.05390 lb/in³ |
| 1.415 g/cc @Temperature 60.0 °C | 0.05112 lb/in³ @Temperature 140 °F |
| 1.434 g/cc @Temperature 50.0 °C | 0.05181 lb/in³ @Temperature 122 °F |
| 1.452 g/cc @Temperature 40.0 °C | 0.05246 lb/in³ @Temperature 104 °F |
| 1.461 g/cc @Temperature 35.0 °C | 0.05278 lb/in³ @Temperature 95.0 °F |
| 1.471 g/cc @Temperature 30.0 °C | 0.05314 lb/in³ @Temperature 86.0 °F |
| 1.48 g/cc @Temperature 25.0 °C | 0.0535 lb/in³ @Temperature 77.0 °F |
| 1.489 g/cc @Temperature 20.0 °C | 0.05379 lb/in³ @Temperature 68.0 °F |
| 1.498 g/cc @Temperature 15.0 °C | 0.05412 lb/in³ @Temperature 59.0 °F |
| 1.508 g/cc @Temperature 10.0 °C | 0.05448 lb/in³ @Temperature 50.0 °F |
| 1.517 g/cc @Temperature 5.00 °C | 0.05481 lb/in³ @Temperature 41.0 °F |
| 1.526 g/cc @Temperature 0.000 °C | 0.05513 lb/in³ @Temperature 32.0 °F |
Viscosity | 0.40 cP @Temperature 60.0 °C | 0.40 cP @Temperature 140 °F |
| 0.43 cP @Temperature 50.0 °C | 0.43 cP @Temperature 122 °F |
| 0.47 cP @Temperature 40.0 °C | 0.47 cP @Temperature 104 °F |
| 0.49 cP @Temperature 35.0 °C | 0.49 cP @Temperature 95.0 °F |
| 0.51 cP @Temperature 30.0 °C | 0.51 cP @Temperature 86.0 °F |
| 0.54 cP @Temperature 25.0 °C | 0.54 cP @Temperature 77.0 °F |
| 0.57 cP @Temperature 20.0 °C | 0.57 cP @Temperature 68.0 °F |
| 0.60 cP @Temperature 15.0 °C | 0.60 cP @Temperature 59.0 °F |
| 0.63 cP @Temperature 10.0 °C | 0.63 cP @Temperature 50.0 °F |
| 0.67 cP @Temperature 5.00 °C | 0.67 cP @Temperature 41.0 °F |
| 0.71 cP @Temperature 0.000 °C | 0.71 cP @Temperature 32.0 °F |
Molecular Weight | 119.4 g/mol | 119.4 g/mol |
Vapor Pressure | 0.0780 bar @Temperature 0.000 °C | 58.5 torr @Temperature 32.0 °F |
| 0.101 bar @Temperature 5.00 °C | 75.8 torr @Temperature 41.0 °F |
| 0.130 bar @Temperature 10.0 °C | 97.5 torr @Temperature 50.0 °F |
| 0.165 bar @Temperature 15.0 °C | 124 torr @Temperature 59.0 °F |
| 0.207 bar @Temperature 20.0 °C | 155 torr @Temperature 68.0 °F |
| 0.258 bar @Temperature 25.0 °C | 194 torr @Temperature 77.0 °F |
| 0.318 bar @Temperature 30.0 °C | 239 torr @Temperature 86.0 °F |
| 0.390 bar @Temperature 35.0 °C | 293 torr @Temperature 95.0 °F |
| 0.475 bar @Temperature 40.0 °C | 356 torr @Temperature 104 °F |
| 0.689 bar @Temperature 50.0 °C | 517 torr @Temperature 122 °F |
| 0.974 bar @Temperature 60.0 °C | 731 torr @Temperature 140 °F |
|
Descriptive Properties |
---|
Appearance | Clear without suspended matter |
Color | <10 |
Composition | <1 mg/kg |
| <5 mg/kg |
| <50 mg/kg |
Purity | >999 g/kg |
Residue on Evaporation | <10 mg/kg |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.