Hostalen PP EBG 252D is a natural, 10 % glass fiber reinforced polypropylene block copolymer (coupled) with high melt viscosity. The product has medium low -temperature impact strength and low thermal coefficient of expansion. The product is used as core layer for the production of 3-layer pipes with reduced thermal elongation. It is not intended for medical and pharmaceutical applications. Applications: Plumbing, Heating & CoolingInformation provided by LyondellBasell. |