Notes: 60GSF6L is a 30% mixed glass sphere and fiber filled nylon 6 that is stabilized for enhanced UV and weathering performance. Availability: Europe Fillers/Reinforcement: Glass Bead\Glass Filler, 30% Filler by Weight Additive: UV Stabilizer Features: Light Stabilized; Weather Resistant Processing Method: Injection Molding Information provided by Teknor Apex |