MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cyclics CBT® 200 Thermoplastic Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between 170-240°C and is available in both one and two-part systems. CBT 200 resin is formulated for various casting, low pressure molding, coating, and composite applications where the lower melt temperature allows for longer working time than CBT 100 resin before polymerizing into PBT.

Information provided by Cyclics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.14 g/ccLiquid (Unpolymerized resin)
Viscosity 11 cP
@Temperature 220 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
 13 cP
@Temperature 210 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
 17 cP
@Temperature 200 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
 22 cP
@Temperature 190 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
 28 cP
@Temperature 180 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
 37 cP
@Temperature 170 °C
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
Linear Mold Shrinkage 0.015 cm/cm
@Thickness 4.00 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 54.0 MPaISO 527
Elongation at Break >= 50 %5 mm/min; ISO 527
Elongation at Yield 3.2 %ISO 527
Tensile Modulus 2.70 GPaISO 527
Flexural Strength 74.0 MPaISO 178
Flexural Modulus 2.38 GPaISO 178
Izod Impact, Notched (ISO) 6.70 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180/U
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 64.0 J/gUnpolymerized resin; ASTM E793
Specific Heat Capacity 1.25 J/g-°CSolid (Unpolymerized resin); ASTM E1269
 1.96 J/g-°C
@Temperature 180 °C
Liquid (Unpolymerized resin); ASTM E1269
Melting Point 165 °CUnpolymerized resin
 225 °CASTM D3418
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 240 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cyclics CBT® 100 Thermoplastic Resin
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
BASF Ultradur® B 2550 PBT
Barlog Plastics KEBAFORM C 901 VT POM Copolymer unreinforced, antistatic

PCYCLIC01 / 29134

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.