MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Insulcast® INSULGEL 50 FC BLACK Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. NSULGEL 50 FC Black is a room temperature curing epoxy gel. It is low in viscosity and does not normally require vacuum de-gassing to assure bubble-free castings.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccUncured. Part B
 1.05 g/ccUncured. Part A
Viscosity 500 cPPart A; ASTM D2393
 500 cPUncured. Part B; ASTM D2393
 550 cPPart A; ASTM D2393
 900 cPUncured. Part B; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength 600 psiASTM D695
Elongation at Break 150 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
cured; ASTM D150
Dielectric Strength 425 V/milASTM D149
Dissipation Factor 0.020ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
Thermal Conductivity 1.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 10.0 min
@Temperature 25.0 °C
Part A
Shelf Life 12.0 MonthPart A
 12.0 MonthPart B
 
Descriptive Properties
Coloramberpart B, uncured
 blackpart A, uncured
Mix Ratio by weight100:25Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9107 / 239617

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.