MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina
Categories: Ceramic; Machinable Ceramic; Oxide; Aluminum Oxide

Material Notes: Partially Fired alumina is machined easily to close tolerances and can be used as-is or fired to increase mechanical and thermal properties. This ceramic offers excellent corrosion, abrasion, wear, and electrical and thermal shock resistance. Used for producing guides, fixtures, nozzles, pump liners, shafts, valve seats, and more. Plates are available from ¼” to ¾” thick × 6” × 6”; rods from ¼” to 3” diameter × 10” long.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.00 g/cc
Water Absorption 25 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 42
Flexural Strength 4000 psi
Compressive Strength 9000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 5.5
@Frequency 1e+6 Hz
Dielectric Strength 80.0 V/mil
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.50 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 30.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 2600 °FOxidizing
Maximum Service Temperature, Inert 1427 °C
 1427 °CVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1550 (Med. Density) Machinable Zirconium Phosphate
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
Crystex Composites Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate

CAREM05 / 546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.