MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ 80XRG 539 Urethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Scotchkote Urethane Elastomer 80XRG 539 has been specifically developed as a fast curing elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.

Product Features:

  • Properties similar to factory produced rubber components
  • Provides good cold vulcanizing capabilities
  • Designed for use to repair conveyer belts, rollers, gaskets, hoses, off road tires etc.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 10.0 MPa1450 psiASTM D412
Elongation at Break 250 %250 %ASTM D412
Tear Strength 51.1 kN/m292 pli
Abrasion 4040[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 50.0 °C122 °FWhite
 80.0 °C176 °FDry
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min0.500 hourInitial Set
 1440 min24.0 hourFull Mechanical
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® TGF2101 + BAYTEC® RG425, 80 A Polyurethane, TDI- PPG
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Isoflon PUR Polyurethane
Taiwan PU Corporation UR80 Polyester Urethane Rubber
SK Chemicals SKYTHANE® 180A R series Polyurethane

PMM35309 / 170056

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.