  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-6712 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Description: LAST-A-FOAM® FR-6700 is a CFC-free, rigid, closed-cell, flame-retardant polyurethane foam for aircraft composite core that withstands process temperatures up to 250°F. It is available in densities ranging from 10 to 25 pounds per cubic foot and exhibits a high strength-to-weight ratio due to its cellular structure and cross-linked resin. Because of its closed-cell structure, LAST-A-FOAM® FR-6700 has great resistance to water absorption and will not swell, crack, or split on exposure to water.

Product Feature:

  • Stable
  • Inert
  • Will not support fungal growth
  • Resistant to most chemicals and solvents
  • Easily shaped with common woodworking tools
  • Performs well as wood replacement
Applications:
  • Models and design prototypes
  • Composite Core
  • Honeycomb edge close-out for aircraft interior sandwich panels used in overhead storage bins, passenger cabin class dividers, galleys and lavatories
  • Vacuum form dies and mold patterns

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.192 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 20.5cut foam surface; ASTM D2240
Tensile Strength 329 psiPerpendicular to Rise; ASTM D1623
 356 psiParallel to Rise; ASTM D1623
Flexural Strength 549 psiRise Parallel to Test Span; ASTM D790
 570 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 18884 psiRise Parallel to Test Span; ASTM D790
 19091 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 225 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 232 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 329 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 330 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 511 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 528 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 766 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 844 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 7466 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 7862 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 9703 psi
@Temperature 93.3 °C
Parallel to Rise; ASTM D1621
 9715 psi
@Temperature 93.3 °C
Perpendicular to Rise; ASTM D1621
 13938 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 15267 psi
@Temperature -53.9 °C
Perpendicular to Rise; ASTM D1621
 15315 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 17554 psi
@Temperature -53.9 °C
Parallel to Rise; ASTM D1621
Poissons Ratio 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°F
@Temperature -45.6 - 93.3 °C
GP Method
Specific Heat Capacity 0.376 BTU/lb-°FASTM E1269
Thermal Conductivity 0.246 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 275 °FASTM E1824
 
Descriptive Properties
Closed Cell Content96.7%
Heat of Combustion10939 BTU/lbASTM D240
Tumbling Friability (%)7.9
Water Absorption0.043 lbs/ft²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3706 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam

PGENR038 / 186824

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.