MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ExxonMobil Exxon™ Bromobutyl 7244 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: White to amber bales.  Slow cure rate grade.

Exxon™ bromobutyl rubber is derived from halogenating butyl rubber with bromine in a continuous process. It is structurally similar to Exxon™ chlorobutyl rubber and produced through the same halogenation process. Bromobutyl rubber grade slate offers a range of polymer viscosities and cure responses, reflecting adjustments in functionality and additives content. Compared with regular butyl rubber, Exxon bromobutyl rubber provides faster and more stable cure through carbon-carbon linking.  Benefits: Low permeability to air, gases and moisture, Low glass transition temperature similar to regular butyl, Wide vulcanization versatility, Fast cure rates, Processing safety: no nitrosamines or nitrosamines precursors.  Exxon bromobutyl rubber is a copolymer of isobutylene and isoprene.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/cc
Mooney Viscosity 41 - 51
@Temperature 125 °C
ML 1+8. MV 200 or equivalent; ASTM D1646
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br 0.930 - 1.13 %ExxonMobil Method
Calcium, Ca 0.14 - 0.20 %ExxonMobil Method
H2O, Water <= 0.30 %ExxonMobil Method
 
Descriptive Properties
Antioxidant (non-staining)0.01 - 0.075wt%. Non-staining. Irganox 1010 ExxonMobil Method
Cure Characteristics14.5 - 23.5dN*m. ML. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).
 38.0 - 52.0dN*m. MH. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod)
 6.0 - 14.0min. t'90. ASTM D2084 (mod). Rheometer ODR 2000 standard compound: ASTM D3958 (mod).
Stabilizer1.0 - 1.6
 Epoxidized soybean oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exxon™ Bromobutyl 2244 Rubber
ExxonMobil Exxon™ Bromobutyl 2235 Rubber
ExxonMobil Exxon™ Bromobutyl 2211 Rubber

PEX98814 / 238199

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.