MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DEMNUM™ S-200 Perfluoropolyether oil
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: DEMNUM™ is a perfluoropolyether oil that has a straight-chain structure developed using DAIKIN’s original technology. It has excellent thermal and chemical stability and inertness, and is suitable as a lubricant grease especially when durability and cleanliness are required. DEMNUM GREASE is a grease formed with DEMNUM as the base oil, chemically inert with excellent high-thermal stability and solvent resistance.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.894 g/cc
Viscosity Measurement 210Index
Kinematic Viscosity 95 cSt
@Temperature 60.0 °C
 500 cSt
@Temperature 20.0 °C
Kinematic Viscosity at 40°C (104°F) 200 cSt
@Temperature 40.0 °C
Kinematic Viscosity at 100°C (212°F) 30 cSt
@Temperature 100 °C
Molecular Weight 8400 g/mol
Vapor Pressure 3.00e-14 bar
@Temperature 20.0 °C
 2.00e-10 bar
@Temperature 100 °C
Surface Tension 19.1 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 72000 V
@Thickness 2.50 mm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.00 J/g-°C
Pour Point -53.0 °C
Glass Transition Temp, Tg -104 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.298nD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin DEMNUM™ S-20 Perfluoropolyether oil
RTP Company RTP 899 X 90822 Acetal (POM), PTFE Lubricated - Perfluoropolyether Oil
Daikin DEMNUM™ S-65 Perfluoropolyether oil
RTP Company RTP 399 X 96252 Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Perfluoropolyether Oil
RTP Company RTP 2299 X 113763 B Polyetheretherketone (PEEK), Carbon Fiber - Aramid Fiber - PTFE Lubricated - Perfluoropolyether Oil

PDAIJ9940 / 210011

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.