MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C18900
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: welding rod and wire for inert gas tungsten arc and metal arc welding and oxyacetylene welding of copper.

Available as rod, wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.89 g/ccSimilar Alloys
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 262 - 655 MPa
Tensile Strength, Yield 62.0 - 359 MPaDepending on temper
Elongation at Break 48 %in 355.6 mm.
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 ohm-cm30% IACS
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 75.0 BTU-in/hr-ft²-°F
Liquidus 1967 °F
Annealing Point 925 - 1100 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 98.75 %
Manganese, Mn 0.20 %
Silicon, Si 0.30 %
Tin, Sn 0.75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 519 Phosphor Bronze 6%, Annealed
Eagle Brass 519 Phosphor Bronze 6%, Hard
Eagle Brass 519 Phosphor Bronze 6%, 3/4 Hard
Eagle Brass 519 Phosphor Bronze 6%, 1/2 Hard
Eagle Brass 519 Phosphor Bronze 6%, 1/4 Hard

MC18900b1 / 10923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.