MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Zr 702 Zirconium
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: In environments where even the best stainless steels are not sufficiently corrosion resistant, titanium, zirconium and tantalum can be used in many applications. Of these titanium is normally the least expensive and tantalum the most corrosion resistant material. Zirconium is in many cases the ideal choice from both technical and economical point of view (the price/life time relation).

Zirconium 702 is characterized by:

  • High heat transfer efficiency
  • Very low thermal expansion
  • Immunity to SCC
  • High resistance to localized (pitting and crevice) forms of corrosion
  • Very good corrosion resistance in most organic acids
  • Exceptional corrosion resistance in mineral acids
  • Good corrosion resistance in strong alkalis
  • Information provided by Sandvik

    ASTM B523

    Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesOriginal ValueComments
    Density 6.50 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate >= 380 MPa
     150 MPa
    @Temperature 350 °C
     390 MPa
    @Temperature 50.0 °C
    Tensile Strength, Yield 75.0 MPa
    @Temperature 350 °C
     250 MPa
    @Temperature 50.0 °C
     >= 205 MPa
    @Strain 0.2 %
    Elongation at Break 16 %2% offset
    Modulus of Elasticity 99.3 GPa
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 5.40 µm/m-°C
    @Temperature 100 °C
    Thermal Conductivity 22.0 W/m-K
    Melting Point 1852 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C <= 0.050 %
    Fe + Cr <= 0.20 %
    Hafnium, Hf <= 4.5 %
    Hydrogen, H <= 0.0040 %
    Nitrogen, N <= 0.020 %
    Oxygen, O 0.125 %
    Zirconium, Zr 94.7 - 99.2 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    ATI Wah Chang Zircadyne® Alloy Zr 702
    Grade 702 Zirconium, Commercially Pure
    Titanium Ti-6Al-4V (Grade 5), Annealed
    Zircaloy-2 Zirconium Alloy
    Aluminum 6061-O

    NSANDV290 / 19184

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.