MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties:
  • Improved toughness as compared to Tuf-Stiff
  • Rigidity/Stiffness
  • Dimensional Stability
  • Durability
  • Colorability
  • Flame retardant
  • Chemical Resistance

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D-785
Hardness, Shore D 80ASTM D-2240
Tensile Strength, Yield 6500 psiASTM D-638
Tensile Modulus 700000 psiASTM D-638
Flexural Strength 12100 psiASTM D-790
Flexural Modulus 700000 psiASTM D-790
Gardner Impact 0.210 ft-lbper mil; ASTM D-4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 µin/in-°F
@Temperature 20.0 °C
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 165 °FASTM D-648
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Zone 1 300 °F
Zone 2 310 °F
Zone 3 320 °F
Zone 4 330 °F
Zone 5 340 °F
Die Temperature 355 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34
Geon® Performance Solutions Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid
Axiall 2512 Rigid PVC, Extrusion
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
Axiall 5006 Rigid PVC, Extrusion, Natural

PGGUL388 / 41664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.