MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KLJ Group 0720 PPO/HIPS, 20% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Key Features: Flame Retardant, 20% Glass Fiber

Applications
Automotive: Fuse and Relay Box, Exterior Body Panel, Electric Vehicle Battery Module Housing, Wheel Covers, Bobbins
Water and Fluid System: Pump Impeller, Pump Housing, Water Softener Tank, Water Purifier Part
Electrical/Electronic: TV Front Cover, TV Rear Cover, TV Stand Base, Speaker Housing, Toner Cartridge Housing, Adapter
Industrial/Household: PV Module Junction Box, Battery Module Housing, Battery Tray, Motor and Generator Cover

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1200 kg(f)/cm²ASTM D638
Flexural Strength 162 MPaASTM D790
Flexural Modulus 62000 kg(f)/cm²ASTM D790
Izod Impact, Notched 7.50 kg-cm/cm
@Temperature -30.0 °C
ASTM D256
 9.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ043 / 284064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.