MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TBA ECP 534 Static Dissipative Powder Coating
Categories: Other Engineering Material

Material Notes: ECP 534 is a static dissipative powder coating based on a carboxylated polyester resin modified with epoxies. Designed where the user requires anti static electrostatic dissipative properties in addition to a superior decorative finish eg, static safe workbenches, racks, trolleys etc, it offers excellent flow, toughness and good chemical resistance. A range of substrates may be coated. Used in the electronics industry where ESD (electro static discharge) is to be avoided.

All tests have been carried out on degreased zinc-phosphated steel coated at 70µmand cured at 10 minutes at 180°C object temperature.

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/cc
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1.00e+9 ohmASTM D257
Static Decay <= 2.0 sec5000V - 50V; JC1155
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 min
@Temperature 200 °C
 10.0 min
@Temperature 180 °C
 20.0 min
@Temperature 160 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Colorlight grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTBA031 / 281509

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.