MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CORFIL® 615 Potting Compound
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Description: CORFIL® 615 potting compound is a low density compound for use as insert or edge filling material in honeycomb sandwich construction. After the curing agent is added, CORFIL 615 remains a thick paste which will not run of its own weight when placed in the desired construction. This thixotropic property is highly convenient because it eliminates the need for molds or other containing devices during the curing period. After CORFIL 615 is cured it will withstand subsequent temperatures up to 350°F (177°C) without becoming fluid or otherwise impairing its use as a structural material. Three curing agents are available to cure the potting compound to a hard, rigid material. These are: Curing Agent “Z” for curing at elevated temperature; Curing Agent “A” for curing at 120°F (49°C); and Curing Agent “DTA” for curing at ambient temperature

Note 1: Curing agent “A” 6 pha, with cure cycle 2 hours at room temperature plus 16 hours at 120°F (49°C)

Note 2: Curing agent “Z” 14.5 pha, with cure cycle 16 hours at 120°F (49°C) plus 1 hour at 300°F (149°C)

Note 3: Curing agent “DTA” 7 pha, with cure cycle 24 hours at room temp.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.600 g/ccAvg, Note 1
 0.547 - 0.686 g/ccNote 1
 0.646 g/ccAvg, Note 3
 0.600 - 0.710 g/ccNote 3
 0.668 g/ccAvg, Note 2
 0.655 - 0.684 g/ccNote 2
Storage Temperature <= 29.0 °C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 91.8 ksiNote 1
 115 ksiNote 3
 218 ksiNote 2
Compressive Strength 3700 - 4440 psiNote 3
 4150 psiAvg, Note 3
 4000 - 7210 psiNote 1
 6000 psiAvg, Note 1
 7625 psiAvg, Note 2
 7500 - 7750 psiNote 2
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorDark Maroon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyimide
CEN® Electronic Material HT Polyimide Film
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
Overview of materials for Polyimide, Thermoset Film
CEN® Electronic Material CF 120CF616 Polyimide Film

PCYTED010 / 180312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.