MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wieland Porta Maximum NF PFM Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Material Notes: All-purpose alloy for low-fusing high expanding ceramics

Applications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneering

Dental

Key Words: EN ISO 1562 or 8891/9693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.4 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 240HV5/30; after porcelain firing
 260HV5/30; hardened
Tensile Strength, Yield 92820 psi
@Strain 0.2 %
after porcelain firing
 101500 psi
@Strain 0.2 %
hardened
Elongation at Break 3.0 %after porcelain firing
 3.0 %hardened
Modulus of Elasticity 110 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 25.0 - 500 °C
Melting Point 1870 - 2030 °F
Solidus 1870 °F
Liquidus 2030 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1470 °FPreheating Temp.
Casting Temperature 2300 °F
 
Component Elements PropertiesOriginal ValueComments
Gold, Au 71 %
Indium, In 2.7 %
Iridium, Ir 0.30 %
Palladium, Pd 11 %
Silver, Ag 13 %
Zinc, Zn 2.0 %
 
Descriptive Properties
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wieland Auropal 1 Casting Alloy
Wieland BioPorta G PFM Alloy
Wieland Porta Maximum PFM Alloy
Wieland Porta P6 PFM Alloy
Wieland Porta REFLEX® PFM Alloy

NWIELAN10 / 19812

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.