MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Main Charactistics: Stress resistant; High impact strength at 196 ° C
Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine Tools

Information provided by Zedex

Key Words: PEEK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Water Absorption 0.050 %
@Temperature 23.0 °C
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.10 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 100DIN 53505
Hardness, Shore D 85DIN 53505
Ball Indentation Hardness 190 MPaDIN 2039
Tensile Strength at Break 98.0 MPaDIN EN ISO 527
Tensile Strength 113 MPaDIN EN ISO 527
Tensile Strength, Yield 78.0 MPaElastic Limit
 113 MPaDIN EN ISO 527
Tensile Stress at Strain 29.0 MPa
@Strain 1 %,
Time 3.60e+6 sec
DIN 53444
Elongation at Break 9.0 %
 9.0 %DIN EN ISO 527
Elongation at Yield 1.3 %Elastic Yield Point
 5.0 %DIN EN ISO 527
 5.0 %Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 4400 MPaDIN EN ISO 527
Flexural Strength 119 MPaOuter Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
 159 MPaDIN EN ISO 178
Flexural Modulus 2937 MPaDIN EN ISO 178
Flexural Strain at Yield 6.6 %DIN EN ISO 178
Compressive Strain at Yield 12.5 %Nominal; DIN EN ISO 604
Compressive Yield Strength 122 MPaElastic Limit
 146 MPaDIN EN ISO 604
Compressive Strength 40.0 MPa
@Time 3.60e+7 sec
 103 MPa
@Time 360000 sec
 130 MPa
@Time 36.0 sec
 36.0 MPa
@Strain 3.5 %
DIN EN ISO 604
Compressive Modulus 2850 MPaDIN EN ISO 604
Fatigue Strength 65.0 MPa
@# of Cycles 1.00e+6
1 Hz
K Factor (ISO) 1.2 µm/km
@Temperature 200 °C
 3.7 µm/km
@Temperature 240 °C
 9.1 µm/km
@Temperature 100 °C
 12 µm/km
@Temperature 20.0 °C
Charpy Impact Unnotched NBEN ISO 179/1eU
Charpy Impact, Notched 6.20 kJ/m²EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.14
@Temperature 20.0 °C
Dry Operation
 0.21
@Temperature 100 °C
Dry Operation
Coefficient of Friction, Static 0.18
@Temperature 20.0 °C
Dry Operation
Tensile Creep Modulus, 1000 hours 2780 MPaAt 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.300 MPa-m/secv = 200m/min
 0.33333 MPa-m/secv = 100m/min
 0.91666 MPa-m/secv = 10m/min
 1.00 MPa-m/secv = 1m/min
Compression Set 8.3 %Elastic Compression Limit
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cmIEC 93
Surface Resistance 7.80e+11 ohmIEC 93
Dielectric Constant 3.0
@Frequency 110 Hz
IEC 250
Dielectric Strength 26.0 kV/mmIEC 243
Dissipation Factor 0.0020IEC 112
 0.053
@Frequency 110 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
@Temperature <=100 °C
ISO E 830
 58.0 µm/m-°C
@Temperature <=150 °C
ISO E 831
Specific Heat Capacity 0.900 J/g-°CDSC
Thermal Conductivity 0.240 W/m-KDIN 52612
Melting Point 340 °CDSC
Maximum Service Temperature, Air 140 °CPressed Bushings
 250 °CContinuous
 260 °CShort Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 165 °CDIN EN ISO 75
Glass Transition Temp, Tg 146 °CDSC
Flammability, UL94 V-0
 
Descriptive Properties
Alignment Adjustment4Nominal Scale: 1, low; 10, high
Chemical Sterilization10Nominal Scale: 1, low; 10, high
ColorBlack
Creep Resistance5Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion5Nominal Scale: 1, low; 10, high
Free from SiliconApplicable
Gamma-rays Radiation Sterilization10Nominal Scale: 1, low; 10, high
High Precision Bushings (negative clearance)Applicable
Injection Molded PartsApplicable
Machined PartsApplicable
Moist Heat Sterilization10Nominal Scale: 1, low; 10, high
Plastic GranulesApplicable
Resistance Against dust, Dirt, Abrasive Substances7Nominal Scale: 1, low; 10, high
Resistance Against Hot Water200
Resistance to Chemicals8Nominal Scale: 1, low; 10, high
Resistant Against DisinfectantApplicable
Rods up to Øe (de)Applicable
ROHS/WEEEApplicable
Sheets up to Maximum ThicknessApplicable
Sliding Velocity100
Suitable for Outdoor Use7Nominal Scale: 1, low; 10, high
Suitable for Use in WaterApplicable
Suitable for VacuumApplicable
Tubes (hollow rods) up to Øe (de)Applicable
UV Rays Resistance9Nominal Scale: 1, low; 10, high
UV-Sterilization7Nominal Scale: 1, low; 10, high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Silicon Nitride/Aluminum Nitride/Aluminum Oxide (Sialon)
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Asahi Kasei Leona™ 53G33 Polyamide 66, Heat Stabilized, GF Reinforced
Asahi Kasei Leona® 1300S Nylon 66
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets

PZEDEX08 / 122123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.