MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Estane® MB ABHU1 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Product Description: Estane® MB ABHU1 is a Polyester TPU base UV stabilizer masterbatch developed for extrusion and molding applications. Incorporation of 2 to 3% Estane® MB ABHU1 in Estane® TPU grades results in molded and extruded articles with an improved UV resistance. To obtain an good dispersion of the UV stabilizer masterbatch in the TPU matrix during extrusion/molding, it is advised a screen pack (up to 100 mesh) during extrusion and sufficient screw back pressure during molding. Recommended to dry MB before processing till + 0.05% moisture.

Availability: Africa & Middle East; Europe; Latin America; North America

Additive: UV Stabilizer

Uses: Masterbatch

Agency Ratings: EC 1907/2006 (REACH)

Processing Method: Extrusion; Injection Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 2781
Maximum Moisture Content 0.050Injection
 0.050Extrusion
 
Processing PropertiesOriginal ValueComments
Melt Temperature 338 - 428 °FInjection
 338 - 428 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBRZ786 / 311479

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.