Introduction: LUPOY PC 1303-10C resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength. Main Characteristics: Medium viscosity, UV stabilizer, Good mold release Applications: Appliances, Outdoor appliance, Automotive components Information provided by LG Chemical |