Kumho-Sunny HCG2510MP PC, 10% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, 10% Glass Filled
Material Notes:
HCG2510MP is high rigidity and high tenacity 10% GF PC resin. It has high stability and super shape resistance property. HCG2510MP is mainly used in mobile phone housing, etc.
Information provided by Shanghai Kumho Sunny Plastics co, Ltd
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
g/cc
0.0452
lb/in³
ASTM D792
Maximum Moisture Content
0.020
0.020
Linear Mold Shrinkage
0.0020
-
0.0040
cm/cm
0.0020
-
0.0040
in/in
ASTM D955
Melt Flow
20
g/10 min
@Load 1.20 kg,
Temperature 300 °C
20
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength
59.0
MPa
8560
psi
ASTM D638
Elongation at Break
9.0 %
9.0 %
ASTM D638
Flexural Strength
98.0
MPa
14200
psi
ASTM D790
Flexural Modulus
3.25
GPa
471
ksi
ASTM D790
Izod Impact, Notched
1.40
J/cm
@Thickness 3.20 mm
2.62
ft-lb/in
@Thickness 0.126 in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
135
°C
275
°F
ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
250
-
270
°C
482
-
518
°F
Middle Barrel Temperature
260
-
280
°C
500
-
536
°F
Front Barrel Temperature
280
-
300
°C
536
-
572
°F
Nozzle Temperature
280
-
290
°C
536
-
554
°F
Melt Temperature
290
-
300
°C
554
-
572
°F
Mold Temperature
100
-
140
°C
212
-
284
°F
Drying Temperature
100
-
120
°C
212
-
248
°F
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Back Pressure
0.300
-
1.00
MPa
43.5
-
145
psi
Screw Speed
20
-
100
rpm
20
-
100
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PKMSN127 / 280979
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.