MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
3D Systems LaserForm® Maraging Steel (A), AGING 2
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Maraging steel fine-tuned for use with ProX® DMP 320 metal 3D printers to produce industrial parts and tool inserts with a combination of high strength and excellent hardness. LaserForm Maraging Steel (A) is formulated and fine-tuned specifically for 3D Systems DMP 320 metal 3D Printers to deliver highest part quality and best part properties.

With properties like 1.2709, this steel is easily heat-treatable in a simple age-hardening process resulting in excellent hardness and strength. LaserForm Maraging Steel (A) has good wear resistance. In regards to post-processing, the material shows good weldability and machinability. LaserForm Maraging Steel (A) is ideal for innovative tool and mold designs including conformal cooling channels for injection molding, die casting and extrusion. The material is also used for high-performance aerospace, automotive and other industrial applications which require high strength and wear resistance.

Classification: Parts built with LaserForm Maraging Steel (A) have a chemical composition that conforms to the compositional requirements of Werkstoff Nr. 1.2709.

Information provided by 3D Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.10 g/ccAbsolute theoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 52 - 58ASTM E18
Tensile Strength, Ultimate 2070 - 2250 MPaVertical direction — Z; ASTM E8M
 2230 - 2290 MPaHorizontal direction — XY; ASTM E8M
Tensile Strength, Yield 1990 - 2150 MPaRp0.2%, Vertical direction - Z; ASTM E8M
 2140 - 2220 MPaRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 1.0 - 3.0 %Vertical direction — Z; ASTM E8M
 3.0 - 7.0 %Horizontal direction — XY; ASTM E8M
Charpy Impact 5.00 - 9.00 JASTM E23
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 20.9 W/m-K
Melting Point 1430 - 1450 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr <= 0.25 %
Cobalt, Co 8.5 - 10 %
Iron, Fe 64.05 - 69.2 %Balance
Manganese, Mn <= 0.15 %
Molybdenum, Mo 4.5 - 5.2 %
Nickel, Ni 17 - 19 %
Phosphorus, P <= 0.010 %
Silicon, Si <= 0.10 %
Sulfur, S <= 0.010 %
Titanium, Ti 0.80 - 1.2 %
 
Descriptive Properties
Surface Roughness4-7µmHorizontal direction (XY)
 5-6µmVertical direction (Z)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Overview of materials for Martensitic
Latrobe Cascade™ P21 Prehardened Die Steel (AISI P21)
3D Systems LaserForm® Maraging Steel (A), AGEING 1 Maraging Steel Material

PAPPR3171 / 239139

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.