MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayfit® 566 Polyurethane Flexible Foam System, 90 Index
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Bayfit 566 is a moldable high resilience (HR) polyurethane flexible foam system.

Properties / Applications: Bayfit 566 is a water-blown (MDI)/polyether based foam system used to manufacture high resilience (HR) cold-cure flex molded foam with medium to high load bearing properties. This system is characterized by good flow behavior in a wide variety of parts. Applications include office furniture, recreational seating, armrests and cushions. Bayfit 566 foam made at indices ranging from 80 to 105 typically passes the requirements of CAL-117 for flame resistance. Foams made at higher indices typically do not. As with any product, use of the Bayfit 566 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.0449 - 0.0529 g/ccMolded
 1.02 g/ccComponent B
 1.24 g/ccComponent A
Viscosity 28 cPComponent A
 1100 cPComponent B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 0.0960 - 0.110 MPa
Elongation at Break 113 - 118 %
Tear Strength 0.900 - 1.00 pli
Compression Set 3.3 - 3.6 %50%
 <= 10 %70%
 
Descriptive Properties
AppearanceDark brown liquidComponent A
 Slighlty hazy liquidComponent B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0109 / 201892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.