System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polyethylene Terephthalate (PET)
;
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Material Notes:
30% Glass Fiber Reinforced, Flame Retardant
Information provided by E-Polymers Co. Ltd.
Key Words:
Poly Ethylene Terephthalate
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.67
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
cm/cm
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
95
ASTM D785
Hardness, Rockwell R
120
ASTM D785
Tensile Strength, Yield
150
MPa
ASTM D638
Elongation at Break
2.3 %
ASTM D638
Flexural Yield Strength
230
MPa
ASTM D790
Flexural Modulus
10.3
GPa
ASTM D790
Izod Impact, Notched
0.800
J/cm
ASTM D256
0.800
J/cm
@Temperature -40.0 °C
ASTM D256
Electrical Properties
Original Value
Comments
Electrical Resistivity
1.00e+15
ohm-cm
IEC 93
Surface Resistance
1.00e+14
ohm
IEC 93
Dielectric Constant
3.8
@Frequency 1e+6 Hz
IEC 250
Dissipation Factor
0.018
@Frequency 1e+6 Hz
IEC 250
Thermal Properties
Original Value
Comments
Melting Point
254
°C
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
245
°C
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
ASTM D648
Flammability, UL94
V-0
Oxygen Index
33 %
ASTM D2863
Processing Properties
Original Value
Comments
Processing Temperature
270
-
290
°C
Mold Temperature
80.0
-
100
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
VICTREX ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Thermx® CG933 NC010 PCT
PEPOLY35 / 36337
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.