MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® UltraPure 1299 MD Water Demineralization Resin
Categories: Polymer; Thermoset

Material Notes: For the demineralization of water in the production of ultra pure water (> 18MOhm*cm at 25°C) Lewatit® UltraPure 1299 MD is a ready-to-use mixed bed comprising a gel type strongly acidic cations exchange resin (SAC, Lewatit UltraPure 1219 MD) and a gel type, strongly basic anion exchange resin (SBA, type I, Lewatit UltraPure 1243 MD), individually with a monodispersed bead size distribution (uniform particles) based on a styrene-divinylbenzene copolymer for the use in working/regenerable and polishing/non-regenerable systems for the production of ultra pure water. The monodisperse beads (uniformity coefficient: max 1.1) are chemically and osmotically highly stable. The optimized kinetics lead to an increased operating capacity and the very low content of fines also results in a low pressure drop compared to ion exchange resins with heterodisperse bead size distribution. Lewatit UltraPure 1299 MD is correspondingly adjusted to the total capacity of the individual components to an equivalent ration of 1:1. The smaller bead size of the SAC contributes to better mixing properties. Lewatit UltraPure 1299 MD is highly regenerated and specially cleaned for meeting the specifications of the semiconductor industry. Leaching of organics from Lewatit UltraPure 1299 MD into the treated water is reduced to a level less than 1.0 ppb, and its resistivity achieves a level higher than 18 MOhm*cm.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 g/cc0.0271 lb/in³
Bead Size 0.330 - 0.430 mm0.0130 - 0.0169 inMean, SAC
 0.600 - 0.700 mm0.0236 - 0.0276 inMean, SBA
Storage Temperature 4.00 - 24.0 °C39.2 - 75.2 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 40.0 °C104 °F
 
Descriptive Properties
AppearanceBrown, translucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8859 / 209251

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.