MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 402 Natural FA PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.

Available in: Europe and North America

Product Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: high impact resistance at low humidity levels, good rigidity, and excellent compression resistance. This grade is particularly suitable for the molding of plastic insulators for railway binding and for extrusion of plates and profiles. Suitable for food contact applications (films, packaging, …). This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183/A
Water Absorption 1.5 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm
Linear Mold Shrinkage, Transverse 0.019 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527 Type 1A
Tensile Strength, Yield 80.0 MPaISO 527 type 1 A
Elongation at Break 60 %ISO 527 Type 1A
Elongation at Yield 8.0 %ISO 527 type 1 A
Tensile Modulus 3100 MPaISO 527 Type 1A
Flexural Strength 120 MPaISO 178
Flexural Modulus 2800 MPaISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO 180/1eA
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Strength 27.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75/Af
Oxygen Index 27 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Feed Temperature 255 - 270 °C
Front Barrel Temperature 270 - 285 °C
Die Temperature 260 - 290 °C
Drying Temperature 80.0 °C
@Time 28800 sec
Moisture Content <= 0.10 %
 
Descriptive Properties
Compression Zone240-260°C
Draw-plate temperatures260-270°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 221 Natural FA PA66, DRY
Domo TECHNYL® A 205F PA66, DRY
Radici Radilon® N66-AFR Nylon 66
Omnia Plastica Akulon® PA 66 - Akulon 66 - Dry
E-Polymers SEPAZ® LA30 PA66 LFT Resin

PRHOD711 / 137942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.