MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Silastic® LSR 9151-200P Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: LSRs for sleeving applications provide a range of elastomers suitable for electrical and thermal protection of wires and cables. These LSRs are available in low to medium viscosities to meet a wide range of processing requirements.

Product applications:

  • Insulation Wrap
  • Protective clothing
Key Features:
  • Good flame retardancy
  • Off-white
  • Two part; 10:1 mix ratio

Former Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
Viscosity 25000 cP
@Frequency 10 Hz
25000 cP
@Frequency 10 Hz
CTM 0050
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength 1.30 MPa189 psiASTM D412
Elongation at Break 200 %200 %ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Silastic® HV 1551-95P LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® LCF 4630 Coating Liquid Silicone Rubber
Dow Silastic® DY-35-3115 Liquid Silicone Rubber
Dow Silastic® 99-595-HC LIQUID SILICONE RUBBER KIT
Dow Silastic® 9390-70 LSR Oil-Resistant Liquid Silicone Rubber

PDOW9953 / 233156

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.