MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Copper Alloy, UNS C10910, M20 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Hot Rolled

Fabrication Properties: Excellent Suitability - Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability - Gas Shielded Arc Welding, Butt Weld; Fair Suitability - Oxyacetylene Welding

Common Fabrication Processes: Blanking; Coining; Coppersmithing; Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot Forming; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical Uses: Busbars; Conductors, Electrical; Telecommunication Cables; Welding and Brazing Components

Applicable Specifications: Bar – ASTM B152/B152M; Sheet, Strip, Roller Bar & Plate – ASME SB152; Strip – ASTM B152/B152M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  50
@Thickness 6.35 mm
50
@Thickness 0.250 in
 62
@Thickness 1.02 mm
62
@Thickness 0.0400 in
Hardness, Rockwell F  40
@Thickness 6.35 mm
40
@Thickness 0.250 in
 45
@Thickness 1.02 mm
45
@Thickness 0.0400 in
Hardness, Rockwell 30T 6464
Tensile Strength  221 MPa
@Thickness 6.35 mm
32000 psi
@Thickness 0.250 in
 234 MPa
@Thickness 1.02 mm
34000 psi
@Thickness 0.0400 in
Tensile Strength, Yield 68.9 MPa10000 psi0.2% Offset
Elongation at Break  45 %
@Thickness 1.02 mm
45 %
@Thickness 0.0400 in
 50 %
@Thickness 6.35 mm
50 %
@Thickness 0.250 in
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Fatigue Strength  75.8 MPa
@Thickness 6.35 mm,
# of Cycles 1.00e+8
11000 psi
@Thickness 0.250 in,
# of Cycles 1.00e+8
 96.5 MPa
@Thickness 1.02 mm,
# of Cycles 1.00e+8
14000 psi
@Thickness 0.0400 in,
# of Cycles 1.00e+8
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Strength  152 MPa
@Thickness 6.35 mm
22000 psi
@Thickness 0.250 in
 159 MPa
@Thickness 1.02 mm
23000 psi
@Thickness 0.0400 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000172 ohm-cm0.00000172 ohm-cm100% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.60 µin/in-°F
@Temperature 68.0 - 392 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 32.6 W/m-K226 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
Annealing Point >= 350 °C>= 662 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 °C356 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.5 %>= 99.5 %
Oxygen, O <= 0.0050 %<= 0.0050 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC10910x4 / 291486

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.