Telcar TL-2657A is a high performance thermoplastic elastomer designed for the industrial/transportation markets. It exhibits a high density and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; High Density; High Hardness; High Specific Gravity; Light Stabilized; Medium Flow Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Grommets; Rubber Replacement; Weatherstripping RoHS Compliant:RoHS Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |