MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Information from Shinkong Synthetic Fibers Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 - 1.33 g/ccASTM D792
Viscosity Test 98 - 102 cm³/gASTM D2857
Melt Index of Compound 25 - 31 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
ASTM Color -2.50 - 0.50[a Value]; JIS Z8722
 -2.00 - 2.0[b Value]; JIS Z8722
 81 - 87[L Value]; JIS Z8722
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 40[µ equ/g]; Zimmer PV07013.4
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 220 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D4019
 
Descriptive Properties
THF Content, ppm<2000Gas Chromatography

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant
Shinkong Synthetic Fibers Shinite® D201 PBT
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity

PSHNK032 / 120802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.