MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/cc
Linear Mold Shrinkage, Flow 0.0035 - 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa
@Temperature 150 °C
 60.0 MPa
@Temperature 120 °C
 75.0 MPa
@Temperature 90.0 °C
 95.0 MPa
@Temperature 60.0 °C
 135 MPa
@Temperature 23.0 °C
Elongation at Break 2.1 %
@Temperature 23.0 °C
 2.4 %
@Temperature 60.0 °C
 3.8 %
@Temperature 90.0 °C
 3.9 %
@Temperature 120 °C
 4.2 %
@Temperature 150 °C
Elongation at Yield 3.5 %
@Temperature 120 °C
 3.7 %
@Temperature 150 °C
Tensile Modulus 220 MPa
@Temperature 150 °C
 3200 MPa
@Temperature 120 °C
 4800 MPa
@Temperature 90.0 °C
 7200 MPa
@Temperature 60.0 °C
 9200 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 35.0 kJ/m²
Charpy Impact, Notched 7.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 400 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 115 °C
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
Vicat Softening Point 245 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.750 mm
Oxygen Index 35 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
Glow Wire Ignition Temperature 900 °C
@Thickness 1.00 mm
 900 °C
@Thickness 2.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latilub 66-20T G/20 PA66, 20% Glass Fiber Reinforced, PTFE Filled
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant

PLATH9707 / 177403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.