MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese SO.F.TER Pibiflex® L 6360 NAT Copolyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Injection Molding Thermoplastic Copolyester Elastomer

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.22 %
@Temperature 23.0 °C,
Time 86400 sec
0.22 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength 34.0 MPa4930 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 0.520 GPa75.4 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Temperature -40.0 °C
1.50 ft-lb/in
@Temperature -40.0 °F
ASTM D256/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+12 ohm-cm
@Temperature 100 °C
>= 1.00e+12 ohm-cm
@Temperature 212 °F
ASTM D257
 >= 1.00e+13 ohm-cm
@Temperature 23.0 °C
>= 1.00e+13 ohm-cm
@Temperature 73.4 °F
ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 219 °C426 °FASTM D3417
Vicat Softening Point 203 °C397 °F120°C/h at 10 N; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index 21 %21 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CB276 Thermoplastic Polyolefin Elastomer
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer
Dow Engage® 8401 Polyolefin Elastomer
Celanese SO.F.TER Laprene® 830.951 TPE
Celanese SO.F.TER Laprene® 830.541 TPE

PSOFS784 / 162248

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.