LNP THERMOCOMP DF0061VI compound is based on Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Non-Brominated, Non-Chlorinated Flame Retardant, Wide Processing Window. Features: High Stiffness,Laser Direct Structuring,Flame Retardant,Circuit Solution,Non-Chlorinated,Non-Brominated,Structural Information provided by SABIC |