MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Lucalen G3710E Anhydride-Modified Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: Lucalen G3710E is a maleic anhydride grafted polyethylene resin with a high thermal stability and good flexibility. Lucalen G3710E is primarily designed to be used as the adhesive layer between the top coat polyethylene and the epoxy layer in a 3-layer coating system with easy processing characteristics. Lucalen G3710E is available in pellet form. Applications: Coatings, Protective, Pipe Coating.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 31.2 lb/ft³ISO 60
Density 0.931 g/ccISO 1183-1
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ISO 868
Tensile Strength, Yield 12.0 MPaISO 527-1,-2
Elongation at Break >= 700 %ISO 527-1,-2
Tensile Modulus 400 MPaISO 527-1,-2
Peel Strength >= 40.0 kN/m
@Temperature 80.0 °C
DIN 30670
 >= 200 kN/m
@Temperature 23.0 °C
DIN 30670
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CISO 11357-3
Vicat Softening Point >= 100 °CA/50N; ISO 306
Brittleness Temperature <= -70.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ISO 15512
 
Descriptive Properties
Processing MethodExtrusion Coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7603 / 219240

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.