MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® S 5128 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 5128 is a food grade, gelular, strongly basic anion exchange resin (type I) based on an acrylic-divinylbenzene copolymer of a special bead size distribution. Due to its acrylic structure, Lewatit S 5128 stands for effective adsorption and desorption of naturally occurring organic substances. Its very high total capacity and outstanding mechanical stability together with the excellent resistance to osmotic shock makes it unique for all demineralization applications especially if a low silica leakage is required. Lewatit S 5128 is especially suitable for:
  • the treatment and demineralization of process water used in the food industry
  • the removal of organic matters (NOM), specially from surface water
If using Lewatit S 5128 to treat the aqueous solutions mentioned above, a special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.730 g/cc0.0264 lb/in³
Density 1.09 g/cc0.0394 lb/in³
Bead Size 0.400 - 1.60 mm0.0157 - 0.0630 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 30.0 °C86.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceWhite, translucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8829 / 209221

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.