MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube
Categories: Polymer; Thermoset; Melamine; Melamine Formaldehyde, Molded, Glass Fiber Filler

Material Notes: Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 - 1.90 g/ccIEC 1212-2 7.2
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 120 MPa
@Diameter >=100 mm
Perpendicular to laminations; IEC 1212-2 4.1
Compressive Strength >= 80.0 MPaAxial; IEC 1212-2 4.2
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance >= 100000 ohm
@Diameter 8.00 - 10.0 mm
After immersion in water; IEC 1212-2 5.2
Dielectric Constant <= 8.0
@Frequency 1e+6 Hz
IEC 1212-2 5.3
Dielectric Breakdown >= 10000 V
@Temperature 90.0 °C,
Time 20.0 sec
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
 >= 10000 V
@Temperature 90.0 °C,
Time 60.0 sec
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Dissipation Factor <= 0.020
@Frequency 1e+6 Hz
IEC 1212-2 5.3
 
Descriptive Properties
Cohesion between layers> 150 MPaIEC 1212-2 4.3, Internal diameter <100 mm
Thermal Endurance130 T.I.IEC 1212-2 7.1
Water Absorption< 5 mg/cm²IEC 1212-2 7.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Perstorp Compounds AMITEC 751 Melamine
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet
Perstorp Compounds Aminel GF Melamine
Perstorp Compounds Aminel FX Melamine

PHIPPE942 / 121946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.