MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV X5745B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B Series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a medium hardness, low density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Medium Hardness; Low Density; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER DBL 5562.30 Color: Black; VAG VW501 23 Color: Black

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Viscosity 280 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 44
@Time 5.00 sec
Extruded; ISO 868
 46
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 435 psiFlow; ISO 37
 624 psiAcross Flow; ISO 37
 580 psi
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air at 168 hr; ISO 188
 636 psi
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air at 168 hr; ISO 188
Tensile Stress at Strain 174 psi
@Strain 100 %
Across Flow; ISO 37
 305 psi
@Strain 100 %
Flow; ISO 37
 174 psi
@Strain 100 %,
Treatment Temp. 135 °C
Across Flow, Change in Air at 1000 hr; ISO 188
 176 psi
@Strain 100 %,
Treatment Temp. 150 °C
Across Flow, Change in Air at 168 hr; ISO 188
Elongation at Break 230 %Flow; ISO 37
 540 %Across Flow; ISO 37
 605 %
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air at 168 hr; ISO 188
 616 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air at 168 hr; ISO 188
Tear Strength 97.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 13 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 26 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 42 %
@Temperature 125 °C,
Time 252000 sec
ISO 815
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers EFLEX® V2045 SEBS/TPV
Chengdu Polyster 4502 High Performance Grade TPV
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

PTEKNQ1210 / 237701

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.