MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SACO AEI THERMODAN® TP543CBU Thermoplastic Polymer
Categories: Polymer; Thermoplastic

Material Notes: Description: TP543CBU has been specially developed to comply with the requirements of BS 7655 Section 6 for types LTS1, 2, 3 and 4; EN 50290-2-27 for type HM2 and HD 604 for type HM4. Cables made with TP543CBU have complied with IEC 332 part 1 and 3 fire tests.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccBS EN ISO 1183-3
Melt Flow 7.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
7.0 g/10 min
@Load 47.6 lb,
Temperature 302 °F
Deformation 35 %
@Temperature 90.0 °C
35 %
@Temperature 194 °F
Hot pressure; IEC 60811-508
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.0 MPa1890 psiIEC 60811-501
 14.595 MPa
@Temperature 100 °C,
Time 605000 sec
2116.8 psi
@Temperature 212 °F,
Time 168 hour
IEC 60811-401
Elongation at Break 170 %170 %IEC 60811-501
 50 %
@Temperature -30.0 °C
50 %
@Temperature -22.0 °F
Thermo; IEC 60811-505
 149.6 %
@Temperature 100 °C,
Time 605000 sec
149.6 %
@Temperature 212 °F,
Time 168 hour
IEC 60811-401
 
Electrical PropertiesMetricEnglishComments
Insulation Resistivity  17.4 Megaohm/1000 m
@Temperature 90.0 °C
57.0 Megaohm/1000 ft
@Temperature 194 °F
BS EN 50395
 2350 Megaohm/1000 m
@Temperature 20.0 °C
7700 Megaohm/1000 ft
@Temperature 68.0 °F
BS EN 50395
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 41 %41 %ASTM D 2863
 
Processing PropertiesMetricEnglishComments
Zone 1 120 °C248 °F
Zone 2 130 °C266 °F
Zone 3 140 °C284 °F
Zone 4 150 °C302 °F
Die Temperature 160 °C320 °F
Head Temperature 160 °C320 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO062 / 249429

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.