Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged often and needs to be repaired. The tape is flexible, and the self-healing property of the mastic helps keep out moisture. Scotch® Mining Tape 31 is approved by MSHA (Mining Safety & Health Administration) as the out jacketing of the 3M™ Mining Cable Splice Kits 3100 Series. The tape is printed with MSHA logo.Information provided by 3M |