MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPE E-2655B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2600 series are super high flow high performance thermoplastic elastomer series, available in BLK, designed for automotive exterior molded applications. Sarlink ME-2655B is a medium hardness, low density, resilient, UV stabilized, super high flow injection molding grade excellent delivering excellent aesthetics with good adhesion to glass with primer.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Low Density; High Flow; Low Specific Gravity; Medium Hardness; Outstanding Surface Finish; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Part; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ISO 1183
Viscosity 139 cP
@Shear Rate 206 1/s,
Temperature 200 °C
139 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ISO 11443
Melt Flow 6.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.4 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  55
@Time 15.0 sec
55
@Time 0.00417 hour
ISO 868
 57
@Time 5.00 sec
57
@Time 0.00139 hour
ISO 868
 60
@Time 1.00 sec
60
@Time 0.000278 hour
ISO 868
Tensile Strength at Break 7.79 MPa1130 psiFlow; ISO 37
 10.5 MPa1520 psiAcross Flow; ISO 37
 11.0 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1600 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 11.4 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1650 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  1.56 MPa
@Strain 100 %
226 psi
@Strain 100 %
Flow; ISO 37
 1.94 MPa
@Strain 100 %
281 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 770 %770 %Flow; ISO 37
 880 %880 %Across Flow; ISO 37
 892 %
@Treatment Temp. 125 °C,
Time 605000 sec
892 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 910 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
910 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
Tear Strength 22.8 kN/m130 pliAcross Flow; ISO 34-1
 22.8 kN/m130 pliFlow; ISO 34-1
Compression Set  17 %
@Temperature 22.8 °C,
Time 79200 sec
17 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 36 %
@Temperature 70.0 °C,
Time 79200 sec
36 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 61 %
@Temperature 90.0 °C,
Time 252000 sec
61 %
@Temperature 194 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °F
Middle Barrel Temperature 175 - 195 °C347 - 383 °F
Front Barrel Temperature 180 - 205 °C356 - 401 °F
Nozzle Temperature 180 - 205 °C356 - 401 °F
Melt Temperature 180 - 205 °C356 - 401 °F
Mold Temperature 15.0 - 40.0 °C59.0 - 104 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1083 / 237574

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.