MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® MT409AHS NC010 PA66-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Toughened, Heat Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccDAM; ISO 1183
Melt Density 0.930 g/cc
@Temperature 290 °C
Water Absorption 1.3 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
 7.2 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 2.10 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.017 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55DS; 50% RH; ISO 2039-2
 65DS; DAM; ISO 2039-2
Hardness, Rockwell R 105DS; 50% RH; ISO 2039-2
 115DS; DAM; ISO 2039-2
Ball Indentation Hardness 60.0 MPaH 358/30; 50% RH; ISO 2039-1
 125 MPaH 358/30; DAM; ISO 2039-1
Tensile Strength, Yield 43.0 MPa50% RH; ISO 527-1/-2
 61.0 MPaDAM; ISO 527-1/-2
Elongation at Break 4.4 %parallel; DAM; ISO 527-3
 25 %Nominal; DAM; ISO 527-1/-2
 >= 50 %Nominal; 50% RH; ISO 527-1/-2
Elongation at Yield 5.0 %DAM; ISO 527-1/-2
 28 %50% RH; ISO 527-1/-2
Tensile Modulus 1100 MPa50% RH; ISO 527-1/-2
 2400 MPaDAM; ISO 527-1/-2
Flexural Strength 53.0 MPa50% RH; ISO 178
 75.0 MPaDAM; ISO 178
Flexural Modulus 1000 MPa50% RH; ISO 178
 2200 MPaDAM; ISO 178
Poissons Ratio 0.38DAM
 0.4550% RH
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 29.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 21.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+12 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+13 ohm50% RH; IEC 62631-3-2
Dielectric Constant 3.4
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.6
@Frequency 100 Hz
DAM; IEC 62631-2-1
 3.7
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 6.6
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 22.0 kV/mm50% RH; IEC 60243-1
 23.0 kV/mmDAM; IEC 60243-1
Dissipation Factor 0.0050
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.012
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.044
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.18
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 600 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.73 J/g-°C
@Temperature 290 °C
Melt
Thermal Conductivity 0.140 W/m-K
@Temperature 290 °C
Melt
Melting Point 262 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 80.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.800 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 29.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 20 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 50.0 - 100 °CInjection
 80.0 °COptimum, Injection
Ejection Temperature 190 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)10VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66-I,,M1G1HNR,S14-020
Max. screw tangential speed (m/s)0.3Injection
Odor Class4VDA 270
Part Marking Code>PA66-I<ISO 11469
PolymerPA66-I
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66-IISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® ST801AHS BK010 PA66-HI
Celanese Zytel® MT409AHS BK010 PA66-I
Celanese Zytel® ST801AHS NC010 PA66-HI
Envalior Durethan® BKV 25 H2.0 LT 904040 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber Reinforced

PDSX5481 / 198121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.