MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite EPIALL 1961B-1 Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/ccASTM D792
Apparent Bulk Density 0.900 g/cc0.0325 lb/in³Powder; ASTM D1895
Water Absorption 0.20 %
@Time 173000 sec
0.20 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiASTM D638
Flexural Strength 148 MPa21500 psiASTM D790
Flexural Modulus 16.0 GPa2320 ksiASTM D790
Compressive Strength 241 MPa35000 psiASTM D695
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength  >= 12.8 kV/mm
@Frequency 60 Hz
>= 325 kV/in
@Frequency 60 Hz
SS, wet
 >= 13.7 kV/mm
@Frequency 60 Hz
>= 348 kV/in
@Frequency 60 Hz
ST, wet
Dissipation Factor 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C8.89 µin/in-°FASTM E831
CTE, linear, Transverse to Flow 32.0 µm/m-°C17.8 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FPost Baked; ASTM D658A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Sumitomo Bakelite EPIALL 1960B-1 Epoxy Molding Compound
Sumitomo Bakelite EPIALL 1914A Epoxy Molding Compound
Sumitomo Bakelite E 3938A Epoxy Molding Compound
Solvay EF5313 Polysiloxane Polymer

PSUMIT151 / 193956

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.