MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS SAN-82TR SAN Resin
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
Melt Flow 40 g/10 min
@Load 10.0 kg,
Temperature 220 °C
40 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 64.1 MPa9300 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Flexural Yield Strength 113.1 MPa16400 psiASTM D790
Flexural Modulus 3.43 GPa497 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 191 - 210 °C375 - 410 °F
Middle Barrel Temperature 204 - 221 °C400 - 430 °F
Front Barrel Temperature 216 - 229 °C420 - 445 °F
Nozzle Temperature 204 - 229 °C400 - 445 °F
Mold Temperature 48.9 - 79.4 °C120 - 175 °F
Drying Temperature 71.1 - 79.4 °C160 - 175 °F
Dry Time 2 - 3 hour2 - 3 hour
Injection Pressure 68.3 - 137 MPa9900 - 19800 psi
Screw Speed 40 - 100 rpm40 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS SAN-80HF High Flow SAN Resin
Overview of materials for Styrene Acrylonitrile (SAN), Molded

PZ9PU73 / 21594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.