MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Altemp® X-750 Nickel-Based superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Precipitation hardenable, high strength up to 1300°F, oxidation resistant up to 1800°F.

Applications: aerospace, heat treatment fixtures, forming tools, extrusion dies.

Key Words: UNS N07750
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.28 g/ccPlate and Sheet
 8.30 g/ccBar and Billet
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C >= 30AMS 5542 annealed and AMS 5598 ages, strip and plate
 >= 32AMS 5542 annealed and AMS 5598 ages, sheet
Tensile Strength, Ultimate <= 896 MPaAMS 5542 annealed, strip and sheet
 >= 1069 MPaAMS 5542 aged, strip and plate
 >= 1103 MPaAMS 5598 aged, strip and plate
 >= 1138 MPaAMS 5542 aged, sheet
 >= 1172 MPaAMS 5598 aged, sheet
Tensile Strength, Yield <= 448 MPa
@Strain 0.2 %
AMS 5542 annealed, sheet
 <= 517 MPa
@Strain 0.2 %
AMS 5598 annealed, sheet
 >= 689 MPa
@Strain 0.2 %
AMS 5542 aged, plate
 >= 724 MPa
@Strain 0.2 %
AMS 5542 aged, sheet
 >= 724 MPa
@Strain 0.2 %
AMS 5598 aged, plate
 >= 793 MPa
@Strain 0.2 %
AMS 5598 aged, sheet
Elongation at Break >= 12 %AMS 5598 aged, strip
 >= 15 %AMS 5542 aged, strip
 >= 18 %AMS 5598 aged, sheet and plate
 <= 18 %AMS 5598 annealed, strip
 <= 20 %AMS 5542 annealed, strip
 >= 20 %AMS 5542 aged, sheet and plate
 <= 35 %AMS 5598 annealed, sheet
 <= 40 %AMS 5542 annealed, sheet
Modulus of Elasticity 214 GPa
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.40 - 1.0 %
Carbon, C <= 0.080 %
Chromium, Cr 14 - 17 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.50 %
Iron, Fe 5.0 - 9.0 %As Remainder
Manganese, Mn <= 1.0 %Max 0.35% for plate and strip
Nickel, Ni >= 70 %Includes Co
Niobium, Nb (Columbium, Cb) 0.70 - 1.2 %
Silicon, Si <= 0.50 %Max 0.35% for plate and strip
Sulfur, S <= 0.010 %
Titanium, Ti 2.25 - 2.75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy X-750
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
ATI Allvac® 718-OP® UNS N07718 Nickel Superalloy
Special Metals INCONEL® Alloy 718
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age

NL1031 / 17799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.