MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-5Al-2.5Fe ISO 5832/X Medical Grade
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Alpha/Beta Titanium Alloy. Characteristics: Corrosion resistance, biocompatibility, amenability to osseointegration, high ratio of fatigue strength to elastic modulus, non-toxic, hypoallergenic. Poor cold-working properties.

Applications: Biomedical/surgical devices such as - Hip endoprotheses, knee joints, spinal implants, dental implants, bone nails, screws and plates.

Key Words: Ti5Al2.5Fe; DIN 3.7110; Tikrutan LT 35
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 900 MPaCentrifugally cast specimen
Tensile Strength, Yield 820 MPa0.2% offset, Centrifugally cast specimen
Elongation at Break 6.0 %Centrifugally cast specimen
Reduction of Area 18 %Centrifugally cast specimen
Tensile Modulus 112 GPaSheet rolled at 850°C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 25epsilonR
 122epsiloni
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°C
@Temperature 200 - 1000 °C
Beta Transus 950 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.5 - 5.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe 2.0 - 3.0 %
Nitrogen, N <= 0.050 %
Oxygen, O <= 0.20 %
Titanium, Ti 92.5 %
 
Descriptive Properties
MicrostructureAl-A9
Room Temperature Phasesa+ß

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium IMI 367 (Ti-6Al-7Nb)
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Implant Grade Titanium Alloy
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Ti-6Al-4V (Grade 5), STA
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

MTP525 / 142963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.